玻璃离子水门汀的临床应用与展望
张楚晗, 王淑君, 韦孟廷, 蒋欣怡, 苏冠宇, 战德松, 付佳乐()   
  1. 中国医科大学口腔医学院,沈阳 110002
    中国医科大学口腔医学院口腔材料学教研室,中国医科大学附属口腔医院修复二科,沈阳 110002
  • 收稿日期:2023-03-19 出版日期:2023-08-01
  • 通信作者: 付佳乐

Clinical application and prospect of glass ionomer cements

Chuhan Zhang, Shujun Wang, Mengting Wei, Xinyi Jiang, Guanyu Su, Desong Zhan, Jiale Fu()   

  1. School of Stomatology, China Medical University, Shenyang 110002, China;
    Department of Dental Materials, the Second Department of Prosthodontics, School and Hospital of Stomatology, China Medical University, Shenyang 110002, China
  • Received:2023-03-19 Published:2023-08-01
  • Corresponding author: Jiale Fu
  • Supported by:
    China Medical University College Students Innovation and Entrepreneurship Training Program(202310159028)
引用本文:

张楚晗, 王淑君, 韦孟廷, 蒋欣怡, 苏冠宇, 战德松, 付佳乐. 玻璃离子水门汀的临床应用与展望[J]. 中华口腔医学研究杂志(电子版), 2023, 17(04): 299-308.

Chuhan Zhang, Shujun Wang, Mengting Wei, Xinyi Jiang, Guanyu Su, Desong Zhan, Jiale Fu. Clinical application and prospect of glass ionomer cements[J]. Chinese Journal of Stomatological Research(Electronic Edition), 2023, 17(04): 299-308.

玻璃离子水门汀(GIC)是一种传统牙科修复材料,因其良好的生物相容性、粘接性和氟释放性等优点,临床应用非常广泛,有巨大发展前景。本文归纳了GIC的化学成分、性质分类及优缺点,系统地总结了GIC的临床应用与注意事项,并对现阶段GIC存在的问题与相关改性研究进行了探讨,以期为未来GIC更好地发展和临床应用提供参考依据。

As a conventional dental restorative material, glass ionomer cement (GIC) has been widely used in clinical practice because of its outstanding properties, such as biocompatibility, adhesion and fluoride release ability, and it has a great development prospect. In this review, the chemical composition, classification, advantages and disadvantages, and the clinical application of glass ionomer cement were systematically summarized. The existing problems and modification researches of GIC were discussed in order to provide a reference for its better development and clinical application.

表1 玻璃离子水门汀(GIC)的性能、临床应用与代表产品
表2 玻璃离子水门汀(GIC)、复合树脂和树脂水门汀的区别
[1]
Sidhu SK, Nicholson JW. A review of glass-ionomer cements for clinical dentistry [J]. J Funct Biomater2016,7(3):16. DOI:10.3390/jfb7030016.
[2]
Wilson AD. Glass-ionomer cement—origins,development and future[J]. Clin Mater1991,7(4):275-282. DOI:10.1016/0267-6605(91)90070-v.
[3]
Mount GJ, Makinson OF. Clinical characteristics of a glass-ionomer cement [J]. Br Dent J1978,145(3):67-71. DOI:10.1038/sj.bdj.4804120.
[4]
Baig MS, Fleming GJ. Conventional glass-ionomer materials:A review of the developments in glass powder,polyacid liquid and the strategies of reinforcement [J]. J Dent2015,43(8):897-912. DOI:10.1016/j.jdent.2015.04.004.
[5]
Nicholson JW, Wilson AD. The effect of storage in aqueous solutions on glass-ionomer and zinc polycarboxylate dental cements [J]. J Mater Sci Mater Med2000,11(6):357-360. DOI:10.1023/a:1008929923531.
[6]
Frankenberger R, García-Godoy F, Lohbauer U,et al. Evaluation of resin composite materials. Part I:in vitro investigations [J]. Am J Dent2005,18(1):23-27.
[7]
Leinfelder KF. Glass ionomers:Current clinical developments [J]. J Am Dent Assoc1993,124(9):62-64. DOI:10.14219/jada.archive.1993.0180.
[8]
Nicholson JW, Sidhu SK, Czarnecka B. Enhancing the mechanical properties of glass-ionomer dental cements:A review [J]. Materials(Basel)2020,13(11):2510. DOI:10.3390/ma13112510.
[9]
Kampanas NS, Antoniadou M. Glass ionomer cements for the restoration of non-carious cervical lesions in the geriatric patient [J]. J Funct Biomater2018,9(3):42. DOI:10.3390/jfb9030042.
[10]
Lohbauer U. Dental glass ionomer cements as permanent filling materials?—Properties,limitations and future trends [J]. Materials2009,3(1):76-96. DOI:10.3390/ma3010076.
[11]
Sidhu SK. Glass-ionomer cement restorative materials:A sticky subject?[J]. Aust Dent J2011,56(Suppl 1):23-30. DOI:10.1111/j.1834-7819.2010.01293.x.
[12]
McLean JW, Nicholson JW, Wilson AD. Proposed nomenclature for glass-ionomer dental cements and related materials [J]. Quintessence Int1994,25(9):587-589.
[13]
Wilson AD, Kent BE. A new translucent cement for dentistry. The glass ionomer cement [J]. Br Dent J1972,132(4):133-135. DOI:10.1038/sj.bdj.4802810.
[14]
Nicholson JW. Chemistry of glass-ionomer cements:A review [J]. Biomaterials1998,19(6):485-494. DOI:10.1016/s0142-9612(97)00128-2.
[15]
de Barra E, Hill RG. Influence of glass composition on the properties of glass polyalkenoate cements. Part Ⅲ:Influence of fluorite content [J]. Biomaterials2000,21(6):563-569. DOI:10.1016/s0142-9612(99)00215-x.
[16]
Forsten L. Fluoride release and uptake by glass-ionomers and related materials and its clinical effect [J]. Biomaterials1998,19(6):503-508. DOI:10.1016/s0142-9612(97)00130-0.
[17]
Prosser HJ, Powis DR, Brant P,et al. Characterization of glass-ionomer cements. 7. The physical properties of current materials [J]. J Dent1984,12(3):231-240. DOI:10.1016/0300-5712(84)90067-8.
[18]
Ching HS, Luddin N, Kannan TP,et al. Modification of glass ionomer cements on their physical-mechanical and antimicrobial properties [J]. J Esthet Restor Dent2018,30(6):557-571. DOI:10.1111/jerd.12413.
[19]
唐卫东,陈敏,唐立. 玻璃离子水门汀在不同粉液比条件下的氟释放[J]. 大连轻工业学院学报2001,20(4):242-244. DOI:10.3969/j.issn.1674-1404.2001.04.003.
[20]
Wan Jusoh WN, Matori KA, Mohd Zaid MH,et al. Incorporation of hydroxyapatite into glass ionomer cement (GIC) formulated based on alumino-silicate-fluoride glass ceramics from waste materials [J]. Materials (Basel)2021,14(4):954. DOI:10.3390/ma14040954.
[21]
Wang Y, Darvell BW. Hertzian load-bearing capacity of a ceramic-reinforced glass ionomer cement stored wet and dry [J]. Dent Mater2009,25(8):952-955. DOI:10.1016/j.dental.2009.02.006.
[22]
Moshaverinia A, Ansari S, Movasaghi Z,et al. Modification of conventional glass-ionomer cements with N-vinylpyrrolidone containing polyacids,nano-hydroxy and fluoroapatite to improve mechanical properties [J]. Dent Mater2008,24(10):1381-1390. DOI:10.1016/j.dental.2008.03.008.
[23]
Najeeb S, Khurshid Z, Zafar MS,et al. Modifications in glass ionomer cements:Nano-sized fillers and bioactive nanoceramics [J]. Int J Mol Sci2016,17(7):1134. DOI:10.3390/ijms17071134.
[24]
Lohbauer U, Frankenberger R, Clare A,et al. Toughening of dental glass ionomer cements with reactive glass fibres [J]. Biomaterials2004,25(22):5217-5225. DOI:10.1016/j.biomaterials.2003.12.027.
[25]
Tanaka CB, Ershad F, Ellakwa A,et al. Fiber reinforcement of a resin modified glass ionomer cement [J]. Dent Mater2020,36(12):1516-1523. DOI:10.1016/j.dental.2020.09.003.
[26]
Moshaverinia A, Roohpour N, Rehman IU. Synthesis and characterization of a novel fast-set proline-derivative-containing glass ionomer cement with enhanced mechanical properties [J]. Acta Biomater2009,5(1):498-507. DOI:10.1016/j.actbio.2008.06.011.
[27]
Khoroushi M, Keshani F. A review of glass-ionomers:From conventional glass-ionomer to bioactive glass-ionomer [J]. Dent Res J(Isfahan)2013,10(4):411-420. DOI:10.4103/1735-3327.118464.
[28]
崔恺,陈吉华,赵三军. 玻璃离子水门汀的研究进展[J]. 牙体牙髓牙周病学杂志2008,18(11):644-647.
[29]
Tyas MJ. Milestones in adhesion:Glass-ionomer cements [J]. J Adhes Dent2003,5(4):259-266.
[30]
Falsafi A, Mitra SB, Oxman JD,et al. Mechanisms of setting reactions and interfacial behavior of a nano-filled resin-modified glass ionomer [J]. Dent Mater2014,30(6):632-643. DOI:10.1016/j.dental.2014.02.025.
[31]
Mickenautsch S, Mount G, Yengopal V. Therapeutic effect of glass-ionomers:An overview of evidence [J]. Aust Dent J2011,56(1):10-15. DOI:10.1111/j.1834-7819.2010.01304.x.
[32]
Bollen AM, Huang G, King G,et al. Activation time and material stiffness of sequential removable orthodontic appliances. Part 1:Ability to complete treatment [J]. Am J Orthod Dentofacial Orthop2003,124(5):496-501. DOI:10.1016/s0889-5406(03)00576-6.
[33]
Seghi RR, Leyva Del Rio D. Biomaterials:Ceramic and adhesive technologies [J]. Dent Clin North Am2019,63(2):233-248. DOI:10.1016/j.cden.2018.11.005.
[34]
de Angelis F, D′arcangelo C, Buonvivere M,et al. Shear bond strength of glass ionomer and resin-based cements to different types of zirconia [J]. J Esthet Restor Dent2020,32(8):806-814. DOI:10.1111/jerd.12638.
[35]
Mandall NA, Hickman J, Macfarlane TV,et al. Adhesives for fixed orthodontic brackets [J]. Cochrane Database Syst Rev2018,4(4):CD002282. DOI:10.1002/14651858.CD002282.pub2.
[36]
Benson PE, Alexander-Abt J, Cotter S,et al. Resin-modified glass ionomer cement vs composite for orthodontic bonding:A multicenter,single-blind,randomized controlled trial [J]. Am J Orthod Dentofacial Orthop2019,155(1):10-18. DOI:10.1016/j.ajodo.2018.09.005.
[37]
Fricker JP. Therapeutic properties of glass-ionomer cements:Their application to orthodontic treatment [J]. Aust Dent J2022,67(1):12-20. DOI:10.1111/adj.12888.
[38]
Berg JH. Glass ionomer cements [J]. Pediatr Dent2002,24(5):430-438.
[39]
Dias AGA, Magno MB, Delbem ACB,et al. Clinical performance of glass ionomer cement and composite resin in ClassⅡ restorations in primary teeth:A systematic review and meta-analysis [J]. J Dent2018,73:1-13. DOI:10.1016/j.jdent.2018.04.004.
[40]
王瑾,程为庄. 玻璃离子水门汀的研究进展[J]. 北京生物医学工程2005,24(2):139-142. DOI:10.3969/j.issn.1002-3208.2005.02.016.
[41]
劳嘉成. 树脂与玻璃离子水门汀充填治疗学龄前儿童乳牙龋蚀的效果[J]. 深圳中西医结合杂志2023,33(5):110-112. DOI:10.16458/j.cnki.1007-0893.2023.05.035.
[42]
陈婉璐,李万蒙,李亚琼,等. 玻璃离子水门汀在老年根面龋患者修复中的应用及对龈沟液炎性因子水平的影响[J]. 中国老年学杂志2023,43(2):358-361. DOI:10.3969/j.issn.1005-9202.2022.02.029.
[43]
尹良胜,池韬,钟素苗. 相邻后牙邻面龋的诊治及其树脂充填效果评价的临床研究[J]. 四川医学2019,40(5):487-490. DOI:10.16252/j.cnki.issn1004-0501-2019.05.12.
[44]
李旭. 银粉玻璃离子水门汀填充修复在恒磨牙邻面龋患者中的应用[J]. 医药论坛杂志2020,41(8):103-106. DOI:CNKI:SUN:HYYX.0.2020-08-028.
[45]
Tolidis K, Boutsiouki C, Gerasimou P. Comparative evaluation of microleakage of a carbomer/fluoroapatite-enhanced glass-ionomer cement on primary teeth restorations [J]. Eur J Paediatr Dent2016,17(3):227-233.
[46]
Francisconi LF, Scaffa PM, de Barros VR,et al. Glass ionomer cements and their role in the restoration of non-carious cervical lesions [J]. J Appl Oral Sci2009,17(5):364-369. DOI:10.1590/s1678-77572009000500003.
[47]
Schwendicke F, Müller A, Seifert T,et al. Glass hybrid versus composite for non-carious cervical lesions:Survival,restoration quality and costs in randomized controlled trial after 3 years [J]. J Dent2021,110:103689. DOI:10.1016/j.jdent.2021.103689.
[48]
马健,邵强,于毅. 不同龈下楔状缺损充填材料对牙龈卟啉单胞菌生物膜形成的影响[J]. 上海口腔医学2020,29(4):375-379. DOI:10.19439/j.sjos.2020.04.008.
[49]
Frencken JE, Leal SC, Navarro MF. Twenty-five-year atraumatic restorative treatment(ART) approach:A comprehensive overview [J]. Clin Oral Investig2012,16(5):1337-1346. DOI:10.1007/s00784-012-0783-4.
[50]
Ruengrungsom C, Palamara JEA, Burrow MF. Comparison of ART and conventional techniques on clinical performance of glass-ionomer cement restorations in load bearing areas of permanent and primary dentitions:A systematic review [J]. J Dent2018,78:1-21. DOI:10.1016/j.jdent.2018.07.008.
[51]
Smales RJ, Yip HK. The atraumatic restorative treatment (ART) approach for the management of dental caries [J]. Quintessence Int2002,33(6):427-432.
[52]
da Mata C, Mckenna G, Anweigi L,et al. An RCT of atraumatic restorative treatment for older adults:5 year results [J]. J Dent2019,83:95-99. DOI:10.1016/j.jdent.2019.03.003.
[53]
Ratnayake J, Veerasamy A, Ahmed H,et al. Clinical and microbiological evaluation of a chlorhexidine-modified glass ionomer cement (GIC-CHX) restoration placed using the atraumatic restorative treatment (ART) technique [J]. Materials (Basel)2022,15(14):5044. DOI:10.3390/ma15145044.
[54]
Chailert O, Banomyong D, Vongphan N,et al. Internal adaptation of resin composite restorations with different thicknesses of glass ionomer cement lining [J]. J Investig Clin Dent2018,9(2):e12308. DOI:10.1111/jicd.12308.
[55]
Ribeiro APD, Sacono NT, Soares DG,et al. Human pulp response to conventional and resin-modified glass ionomer cements applied in very deep cavities [J]. Clin Oral Investig2020,24(5):1739-1748. DOI:10.1007/s00784-019-03035-3.
[56]
Mount GJ. Esthetics with glass-ionomer cements and the "sandwich" technique [J]. Quintessence Int1990,21(2):93-101.
[57]
南晓红,寇继寅,李茹. 玻璃离子水门汀的应用及发展[J]. 口腔医学2007,27(6):323-325. DOI:10.3969/j.issn.1003-9872.2007.06.016.
[58]
Manihani AKDS, Mulay S, Beri L,et al. Effect of total-etch and self-etch adhesives on the bond strength of composite to glass-ionomer cement/resin-modified glass-ionomer cement in the sandwich technique—A systematic review [J]. Dent Res J (Isfahan)2021,18:72. DOI:10.4103/1735-3327.326645.
[59]
Sikka N, Brizuela M. Glass Ionomer Cement [M]. Treasure Island (FL):StatPearls,2023.
[60]
Hassani Katehsari V, Niedermeier W. Solubility of dental core build-up materials in electric fields [J]. J Dent Sci2019,14(4):346-351. DOI:10.1016/j.jds.2019.04.005.
[61]
Souza JCM, Fernandes V, Correia A,et al. Surface modification of glass fiber-reinforced composite posts to enhance their bond strength to resin-matrix cements:An integrative review [J]. Clin Oral Investig2022,26(1):95-107. DOI:10.1007/s00784-021-04221-y.
[62]
Li XJ, Zhao SJ, Niu LN,et al. Effect of luting cement and thermomechanical loading on retention of glass fibre posts in root canals [J]. J Dent2014,42(1):75-83. DOI:10.1016/j.jdent.2013.10.017.
[63]
刘莹,王富,赵三军,等. 3种粘结材料对粘结纤维桩的临床疗效观察[J]. 牙体牙髓牙周病学杂志2016,26(2):110-114. DOI:10.15956/j.cnki.chin.j.conserv.dent.2016.02.012.
[64]
Kantovitz KR, Pascon FM, Nociti FH Jr,et al. Inhibition of enamel mineral loss by fissure sealant:An in situ study [J]. J Dent2013,41(1):42-50. DOI:10.1016/j.jdent.2012.09.015.
[65]
Yengopal V, Mickenautsch S, Bezerra AC,et al. Caries-preventive effect of glass ionomer and resin-based fissure sealants on permanent teeth:A meta analysis [J]. J Oral Sci2009,51(3):373-382. DOI:10.2334/josnusd.51.373.
[66]
Markovic D, Peric T, Petrovic B. Glass-ionomer fissure sealants:Clinical observations up to 13 years [J]. J Dent2018,79:85-89. DOI:10.1016/j.jdent.2018.10.007.
[67]
李一涵,王菲,吴珺华. 影响玻璃离子水门汀粘接强度的因素[J]. 广东牙病防治2015,23(1):48-51. DOI:CNKI:SUN:GDYB.0.2015-01-019.
[68]
胡菁颖,李莉,周倩妹,等. 不同调拌板对玻璃离子水门汀物理性能的影响[J]. 北京大学学报(医学版)2019,51(5):964-967. DOI:10.19723/j.issn.1671-167x.2019.05.029.
[69]
叶慧铭,朱曼群,林桂珍,等. 玻璃离子水门汀粘固前牙全冠的调拌方法探讨[J]. 广东牙病防治2012,20(8):441-442. DOI:CNKI:SUN:GDYB.0.2012-08-014.
[70]
邱韬,陈欣蕾,黄娟,等. 调拌方式对玻璃离子水门汀充填体抗压强度的影响[J]. 中国医药导报2019,16(24):111-114. DOI:CNKI:SUN:YYCY.0.2019-24-030.
[71]
邱韬,毛渤淳,张家愚,等. 调拌方式对玻璃离子水门汀充填体边缘微渗漏的影响[J]. 中国医药导报2019,16(33):100-102+115. DOI:CNKI:SUN:YYCY.0.2019-33-025.
[72]
Mar B, Ekambaram M, Li KC,et al. The influence of saliva and blood contamination on bonding between resin-modified glass ionomer cements and resin composite [J]. Oper Dent2023,48(2):218-225. DOI:10.2341/21-173-L.
[73]
Shimazu K, Karibe H, Oguchi R,et al. Influence of artificial saliva contamination on adhesion in class V restorations [J]. Dent Mater J2020,39(3):429-434. DOI:10.4012/dmj.2019-032.
[74]
赵信义. 口腔材料学[M]. 6版. 北京:人民卫生出版社,2020:66-67.
[75]
黄梓濡,邹华,侯沐明,等. 粉液比例对树脂加强型玻璃离子托槽粘接的影响[J/OL]. 中华口腔医学研究杂志(电子版)2015,9(4):301-304. DOI:10.3877/cma.j.issn.1674-1366.2015.04.008.
[76]
Millett DT, Cattanach D, Mcfadzean R,et al. Laboratory evaluation of a compomer and a resin-modified glass ionomer cement for orthodontic bonding [J]. Angle Orthod1999,69(1):58-63. DOI:10.1043/0003-3219(1999)069<0058:LEOACA>2.3.CO;2.
[77]
Hao Y, Huang X, Zhou X,et al. Influence of dental prosthesis and restorative materials interface on oral biofilms [J]. Int J Mol Sci2018,19(10):3157. DOI:10.3390/ijms19103157.
[78]
Fukuda R, Yoshida Y, Nakayama Y,et al. Bonding efficacy of polyalkenoic acids to hydroxyapatite,enamel and dentin [J]. Biomaterials2003,24(11):1861-1867. DOI:10.1016/s0142-9612(02)00575-6.
[79]
Yoshida Y, Van Meerbeek B, Nakayama Y,et al. Evidence of chemical bonding at biomaterial-hard tissue interfaces [J]. J Dent Res2000,79(2):709-714. DOI:10.1177/00220345000790020301.
[80]
Yoshihara K, Nagaoka N, Hayakawa S,et al. Chemical interaction of glycero-phosphate dimethacrylate(GPDM) with hydroxyapatite and dentin [J]. Dent Mater2018,34(7):1072-1081. DOI:10.1016/j.dental.2018.04.003.
[81]
Hasan AMHR, Sidhu SK, Nicholson JW. Fluoride release and uptake in enhanced bioactivity glass ionomer cement ( "glass carbomerTM" ) compared with conventional and resin-modified glass ionomer cements [J]. J Appl Oral Sci2019,27:e2018 0230. DOI:10.1590/1678-7757-2018-0230.
[82]
Patil SS, Kontham UR, Kontham RK,et al. Fluoride release and fluoride-recharging ability of three different sealants [J]. J Indian Soc Pedod Prev Dent2020,38(3):247-252. DOI:10.4103/JISPPD.JISPPD_345_19.
[83]
Bueno LS, Borges AFS, Navarro MFL,et al. Determination of chemical species of fluoride during uptake mechanism of glass-ionomer cements with NMR spectroscopy [J]. Dent Mater2021,37(7):1176-1182. DOI:10.1016/j.dental.2021.04.011.
[84]
Burgess JO, Vaghela PM. Silver diamine fluoride:A successful anticarious solution with limits [J]. Adv Dent Res2018,29(1):131-134. DOI:10.1177/0022034517740123.
[85]
González-Cabezas C, Fernández CE. Recent advances in remineralization therapies for caries lesions [J]. Adv Dent Res2018,29(1):55-59. DOI:10.1177/0022034517740124.
[86]
Ten Cate JM, Buzalaf MAR. Fluoride mode of action:Once there was an observant dentist [J]. J Dent Res2019,98(7):725-730. DOI:10.1177/0022034519831604.
[87]
Walsh T, Worthington HV, Glenny AM,et al. Fluoride toothpastes of different concentrations for preventing dental caries [J]. Cochrane Database Syst Rev2019,3(3):CD007868. DOI:10.1002/14651858.CD007868.pub3.
[88]
Tian KV, Chass GA, Di Tommaso D. Simulations reveal the role of composition into the atomic-level flexibility of bioactive glass cements [J]. Phys Chem Chem Phys2016,18(2):837-845. DOI:10.1039/c5cp05650k.
[89]
Pedone A, Chen X, Hill RG,et al. Molecular Dynamics Investigation of Halide-Containing Phospho-Silicate Bioactive Glasses [J]. J Phys Chem B2018,122(11):2940-2948. DOI:10.1021/acs.jpcb.8b00547.
[90]
Francois P, Fouquet V, Attal JP,et al. Commercially available fluoride-releasing restorative materials:A review and a proposal for classification [J]. Materials(Basel)2020,13(10):2313. DOI:10.3390/ma13102313.
[91]
Dasgupta S, Saraswathi MV, Somayaji K,et al. Comparative evaluation of fluoride release and recharge potential of novel and traditional fluoride-releasing restorative materials:An in vitro study [J]. J Conserv Dent2018,21(6):622-626. DOI:10.4103/JCD.JCD_338_18.
[92]
Garoushi S, Vallittu PK, Lassila L. Characterization of fluoride releasing restorative dental materials [J]. Dent Mater J2018,37(2):293-300. DOI:10.4012/dmj.2017-161.
[93]
Hurle K, Oliveira JM, Reis RL,et al. Ion-doped brushite cements for bone regeneration [J]. Acta Biomater2021,123:51-71. DOI:10.1016/j.actbio.2021.01.004.
[94]
Bermúdez-Reyes B, Del Refugio Lara-Banda M, Reyes-Zarate E,et al. Effect on growth and osteoblast mineralization of hydroxyapatite-zirconia (HA-ZrO2) obtained by a new low temperature system [J]. Biomed Mater2018,13(3):035001. DOI:10.1088/1748-605X/aaa3a4.
[95]
Van Duinen RN, Davidson CL, De Gee AJ,et al. In situ transformation of glass-ionomer into an enamel-like material [J]. Am J Dent2004,17(4):223-227.
[96]
De Caluwé T, Vercruysse CWJ, Ladik I,et al. Addition of bioactive glass to glass ionomer cements:Effect on the physico-chemical properties and biocompatibility[J]. Dent Mater2017,33(4):e186-e203. DOI:10.1016/j.dental.2017.01.007.
[97]
Bossù M, Saccucci M, Salucci A,et al. Enamel remineralization and repair results of Biomimetic Hydroxyapatite toothpaste on deciduous teeth:An effective option to fluoride toothpaste [J]. J Nanobiotechnology2019,17(1):17. DOI:10.1186/s12951-019-0454-6.
[98]
Karimi M, Hesaraki S, Alizadeh M,et al. Effect of synthetic amorphous calcium phosphate nanoparticles on the physicochemical and biological properties of resin-modified glass ionomer cements [J]. Mater Sci Eng C Mater Biol Appl2019,98:227-240. DOI:10.1016/j.msec.2018.12.129.
[99]
Kheur M, Kantharia N, Lakha T,et al. Correction To:Evaluation of mechanical and adhesion properties of glass ionomer cement incorporating nano-sized hydroxyapatite particles[J]. Odontology2020,108(1):152. DOI:10.1007/s10266-019-00434-6.
[100]
Kunte S, Shah SB, Patil S,et al. Comparative evaluation of compressive strength and diametral tensile strength of conventional glass ionomer cement and a glass hybrid glass ionomer cement [J]. Int J Clin Pediatr Dent2022,15(4):398-401. DOI:10.5005/jp-journals-10005-2407.
[101]
Kheur M, Kantharia N, Lakha T,et al. Evaluation of mechanical and adhesion properties of glass ionomer cement incorporating nano-sized hydroxyapatite particles [J]. Odontology2020,108(1):66-73. DOI:10.1007/s10266-019-00427-5.
[102]
Lee JJ, Lee YK, Choi BJ,et al. Physical properties of resin-reinforced glass ionomer cement modified with micro and nano-hydroxyapatite [J]. J Nanosci Nanotechnol2010,10(8):5270-5276. DOI:10.1166/jnn.2010.2422.
[103]
Sun L, Yan Z, Duan Y,et al. Improvement of the mechanical,tribological and antibacterial properties of glass ionomer cements by fluorinated graphene [J]. Dent Mater2018,34(6):e115-e127. DOI:10.1016/j.dental.2018.02.006.
[104]
Dionysopoulos D, Tolidis K, Tortopidis D,et al. Effect of a calcium chloride solution treatment on physical and mechanical properties of glass ionomer cements [J]. Odontology2018,106(4):429-438. DOI:10.1007/s10266-018-0338-5.
[105]
Perera D, Yu SCH, Zeng H,et al. Acid resistance of glass ionomer cement restorative materials[J]. Bioengineering(Basel)2020,7(4):150. DOI:10.3390/bioengineering7040150.
[106]
Mustafa R, Alshali RZ, Silikas N. The effect of desiccation on water sorption,solubility and hygroscopic volumetric expansion of dentine replacement materials [J]. Dent Mater2018,34(8):e205-e213. DOI:10.1016/j.dental.2018.05.012.
[107]
Pitel ML. Long-term performance of glass-hybrid restorations in permanent posterior teeth [J]. Compend Contin Educ Dent2021,42(Suppl 1):6-9.
[108]
Scott JM, Mahoney EK. Restoring proximal lesions in the primary dentition:Is glass ionomer cement the material of choice?[J]. N Z Dent J2003,99(3):65-71.
[109]
Almuhaiza M. Glass-ionomer cements in restorative dentistry:A critical appraisal [J]. J Contemp Dent Pract2016,17(4):331-336. DOI:10.5005/jp-journals-10024-1850.
[110]
Oz FD, Meral E, Ergin E,et al. One-year evaluation of a new restorative glass ionomer cement for the restoration of non-carious cervical lesions in patients with systemic diseases:A randomized,clinical trial [J]. J Appl Oral Sci2020,28:e20200311. DOI:10.1590/1678-7757-2020-0311.
[111]
Gurgan S, Kutuk ZB, Ergin E,et al. Four-year randomized clinical trial to evaluate the clinical performance of a glass ionomer restorative system [J]. Oper Dent2015,40(2):134-143. DOI:10.2341/13-239-C.
[112]
Gurgan S, Kutuk ZB, Ergin E,et al. Clinical performance of a glass ionomer restorative system:A 6-year evaluation [J]. Clin Oral Investig2017,21(7):2335-2343. DOI:10.1007/s00784-016-2028-4.
[113]
Hickel R, Kaaden C, Paschos E,et al. Longevity of occlusally-stressed restorations in posterior primary teeth [J]. Am J Dent2005,18(3):198-211.
[114]
Bijle MN, Ekambaram M, Lo ECM,et al. Antibacterial and mechanical properties of arginine-containing glass ionomer cements [J]. Dent Mater2020,36(9):1226-1240. DOI:10.1016/j.dental.2020.05.012.
[115]
Hafshejani TM, Zamanian A, Venugopal JR,et al. Antibacterial glass-ionomer cement restorative materials:A critical review on the current status of extended release formulations [J]. J Control Release2017,262:317-328. DOI:10.1016/j.jconrel.2017.07.041.
[116]
朱可石,任利玲. 纳米填料改性玻璃离子水门汀的研究进展[J]. 口腔医学研究2022,38(1):13-16. DOI:10.13701/j.cnki.kqyxyj.2022.01.003.
[117]
Zhu K, Zheng L, Xing J,et al. Mechanical,antibacterial,biocompatible and microleakage evaluation of glass ionomer cement modified by nanohydroxyapatite/polyhexamethylene biguanide [J]. Dent Mater J2022,41(2):197-208. DOI:10.4012/dmj.2021-096.
[118]
张宜爽,陶地豪,郭安迪,等. 玻璃离子水门汀天然抗菌成分研究进展[J]. 口腔疾病防治2022,30(10):751-756. DOI:10.12016/j.issn.2096-1456.2022.10.011.
[119]
Yudovin-Farber I, Beyth N, Nyska A,et al. Surface characterization and biocompatibility of restorative resin containing nanoparticles [J]. Biomacromolecules2008,9(11):3044-3050. DOI:10.1021/bm8004897.
[120]
Saghir A, Rehman T, Irum B,et al. 12 Month′s assessment of clinical efficacy of resin modified glass ionomer cement and flowable composites in restoration of non-carious cervical lesions,a randomized clinical trial [J]. J Ayub Med Coll Abbottabad2023,35(1):7-10. DOI:10.55519/JAMC-01-10780.
[121]
Uzel I, Gurlek C, Kuter B,et al. Caries-preventive effect and retention of glass-ionomer and resin-based sealants:A randomized clinical comparative evaluation [J]. Biomed Res Int2022:7205692. DOI:10.1155/2022/7205692.
[122]
Chadwick BL, Evans DJ. Restoration of classⅡ cavities in primary molar teeth with conventional and resin modified glass ionomer cements:A systematic review of the literature [J]. Eur Arch Paediatr Dent2007,8(1):14-21. DOI:10.1007/BF03262565.
[123]
巴晓兰,程为庄. 改性玻璃离子水门汀的研究进展[J]. 生物医学工程学杂志2005,22(4):857-859. DOI:10.3321/j.issn:1001-5515.2005.04.049.
[1] 孙瑞瞳, 李享宜, 胡一淳, 高嘉阳, 胡博, 战德松, 付佳乐. 硅基陶瓷的临床应用现状与展望[J]. 中华口腔医学研究杂志(电子版), 2021, 15(02): 72-78.
[2] 李轲, 郑适泽, 陈玥, 鄢晓媛, 战德松, 付佳乐. 树脂水门汀与氧化锆陶瓷剪切粘接强度的研究[J]. 中华口腔医学研究杂志(电子版), 2019, 13(04): 212-217.
[3] 林双, 黄艳苓, 王晓晴, 刘永灏, 张磊, 战德松, 付佳乐. 树脂水门汀的临床应用进展[J]. 中华口腔医学研究杂志(电子版), 2018, 12(06): 379-382.
[4] 谢丹丹, 麦穗, 吴倩, 赵曼多, 谭易, 古丽莎. 氧化海藻酸钠预处理提高树脂牙本质粘接的耐久性[J]. 中华口腔医学研究杂志(电子版), 2018, 12(06): 329-334.
[5] 黄沁, 杨博, 杨家俊, 霍兆麟, 王焱. 固化模式对双固化树脂水门汀微观机械性能及聚合程度的影响[J]. 中华口腔医学研究杂志(电子版), 2018, 12(04): 199-204.
阅读次数
全文


摘要